Polymer Property : Adhesive Bond Strength = 1110 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 7.65 MPa
1110 psi
Lap shear, alum to alum
Tra-Con Tra-Duct 29121 Snap Cure Conductive Silver Epoxy Adhesive
TRA-DUCT 29121 is 100% solids, two component silver filled epoxy designed for chip bonding in microelectronic and optoelectronic applications. TRA-DUCT 29121 is a soft, smooth paste. This two-part f..