Polymer Property : Adhesive Bond Strength = 1.59 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 1.59 MPa
230 psi
Lap shear, alum to alum, 1 hr @ 65°C
Tra-Con Tra-Duct 2921 Silver-Filled Adhesive
Information provided by Tra-Con Inc.
Adhesive Bond Strength 1.59 MPa
230 psi
Lap shear, alum to alum, 1 hr @ 100°C
Tra-Con Tra-Duct 2929 Room Temperature Conductive Flexible Silver Epoxy Adhesive
TRA-DUCT 2929 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy a..