Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 1.03 MPa | 150 psi | Shear, at 100% cohesive failure |
Momentive Performance Materials IS808 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Translucent IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Adhesive Bond Strength | 1.03 MPa | 149 psi | Typical lap shear |
Momentive Performance Materials RTV102 White Adhesive Sealant, High Strength Paste One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: High strength high perfo.. |
|||
Adhesive Bond Strength | 1.03 MPa | 149 psi | Typical lap shear |
Momentive Performance Materials RTV103 Black Adhesive Sealant, High Strength Paste One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: High strength high perfo.. |
|||
Adhesive Bond Strength | 1.03 MPa | 149 psi | Typical lap shear |
Momentive Performance Materials RTV108 Translucent Adhesive Sealant, High Strength Paste One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: High strength high perfo.. |
|||
Adhesive Bond Strength | 1.03 MPa | 149 psi | Typical lap shear |
Momentive Performance Materials RTV109 Aluminum Adhesive Sealant, High Strength Paste One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: High strength high perfo.. |
|||
Adhesive Bond Strength | 1.03 MPa | 149 psi | Typical lap shear |
Momentive Performance Materials RTV162 White Adhesive Sealant, Non-Corrosive Paste One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Non-corrosive bindi.. |
|||
Adhesive Bond Strength | 1.03 MPa | 150 psi | Shear, at 100% cohesive failure |
Momentive Performance Materials IS800.09 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Aluminum IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Adhesive Bond Strength | 1.03 MPa | 150 psi | Shear, at 100% cohesive failure |
Momentive Performance Materials IS802 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, White IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Adhesive Bond Strength | 1.03 MPa | 150 psi | Shear, at 100% cohesive failure |
Momentive Performance Materials IS803 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Black IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |