Polymer Property : Adhesive Bond Strength = 0.0228 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.0228 MPa
3.30 psi
Arlon SQA-TMS-011
Arlon 18976XA023 Silicone Rubber/Fiberglass Laminate
Side 1:cured silicone rubber; Substrate: 11523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene