Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.0214 MPa
3.10 psi
Arlon SQA-TMS-011
Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber
Adhesive Bond Strength 0.0214 MPa
3.10 psi
MIL-I-46852C
Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape
1 inch wide, 20 mil thick, Red, Rectangular cross-section self-fusing silicone tape. Meets U.S. Military Specification A-A-59163 (supercedes Mil-I-46852C) except for packaging and sampling. The foll..