Polymer Property : 2% Secant Modulus = 61.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.421 GPa
61.0 ksi
0.5 in/min; ASTM D790
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade
ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow..