Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.140 GPa | 20.3 ksi | TD; ASTM D882 |
Braskem CX7020 Cast Film Extrusion Low Density Polyethylene Smooth or embossed films for diapers, disposable sheets, etc. Films for lamination, Injection-Blow Molding, Foamed applications.Information provided by Braskem. |