Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 1.10 GPa | 160 ksi | 500mm/min; ASTM D638 |
LG Chemical SEETEC BF500 LDPE Characteristics: Good Processability and Good Optical Properties Additives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chem.. |
|||
2% Secant Modulus | 1.10 GPa | 160 ksi | 500mm/min; ASTM D638 |
LG Chemical SEETEC BS500 LDPE Characteristics: Good Processability and Good cell uniformity& stability Additives: Antioxidant, Antiblocking agent, Slip AgentApplications: Foam sheetInformation provided by LG Chemical |