Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.0351 GPa | 5.09 ksi | ASTM D790 |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |