Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 40.7 J @Temperature -40.0 °C |
30.0 ft-lb @Temperature -40.0 °F |
|
Universal Wire Works E81T1-Ni2 Flux Cored Carbon Steel Tubular Electrode Alloys 81T1-Ni1 and Ni2 are designed for gas-shielded flux cored welding of low alloy steels that require good CVN toughness at subzero temperatures. These alloys are excellent for single and multip.. |
|||
Charpy Impact | 40.7 J | 30.0 ft-lb | |
Wingate Alloys Winco-Tuf 40IT Ultra High Strength, Thru-Hardened Alloy Wear Plate For extreme abrasion and moderate impact.Winco-Tuf 40 has excellent toughness at high hardness and in heavy sections. For severe impact and abrasions.Advantages: Maximum resistance to abrasion and i.. |
|||
Charpy Impact | 40.7 J @Temperature -28.9 °C |
30.0 ft-lb @Temperature -20.0 °F |
|
Universal Wire Works E81T1-Ni1 Flux Cored Carbon Steel Tubular Electrode Alloys 81T1-Ni1 and Ni2 are designed for gas-shielded flux cored welding of low alloy steels that require good CVN toughness at subzero temperatures. These alloys are excellent for single and multip.. |
|||
Charpy Impact | 40.7 J @Treatment Temp. 1070 °C |
30.0 ft-lb @Treatment Temp. 1950 °F |
austenitizied at 1950°F; C-notch |
Crucible Steel CRU-WEAR® Tool Steel CRU-WEAR is an air-hardening tool steel, heat treatable to HRC 60-65. Designed as an upgrade to D2, it offers better wear resistance, greater toughness and higher attainable hardness. Compared to th.. |
|||
Charpy Impact | 40.7 J | 30.0 ft-lb | notched |
Carpenter AerMet® 100 Aged at 875°F An alloy providing high hardness and strength combined with exceptional ductility and toughness. This alloy should be considered for aircraft and aerospace structural components requiring high stren.. |