Polymer Property : Charpy Impact = 25.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 33.9 J
25.0 ft-lb
496°C Temper Temperature
Latrobe Lescalloy® 16NCD13 VAC-ARC High Strength Alloy Steel
16NCD13 VAC-ARC is a premium quality low alloy, carburizing casehardenable vacuum arc remelted steel which takes its name from the French industry designation. In the carburized condition, its high ..
Charpy Impact 33.9 J
25.0 ft-lb
V-Notch; Air Cooled from 1010°C; 172°C Temper Temperature
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12)
TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste..
Charpy Impact 33.9 J
25.0 ft-lb
V-Notch; Air Cooled from 1010°C; 370 Temper Temperature
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11)
TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides..
Charpy Impact 33.9 J
25.0 ft-lb
V-Notch
ECOMold 135 Copper Mold Material
ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. T..
Charpy Impact 33.9 J

@Temperature 20.0 °C
25.0 ft-lb

@Temperature 68.0 °F
Age hardened at 42 HRC
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel
Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, ..
Charpy Impact 33.9 J

@Temperature 20.0 °C
25.0 ft-lb

@Temperature 68.0 °F
Age hardened at 42 HRC
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel
Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, unifor..
Charpy Impact >= 33.9 J

@Thickness >=3.17 mm
>= 25.0 ft-lb

@Thickness >=0.125 in
transverse
American Utility Metals 3CR12® Stainless Steel
3CR12 is a weldable ferritic stainless steel, specifically designed for aggressive material handling applications. It is intended to provide the benefits of traditional stainless steel, such as stre..
Charpy Impact 33.9 J
25.0 ft-lb
Notched; at 38 HRC
Schmolz + Bickenbach Formadur® PH X Superclean Plastic Mold Steel
Description: Formadur® PH X Superclean is a corrosion-resistant, martensitic precipitation hardened stainless steelCharacteristics: Excellent resistance to corrosion; Excellent polishability; Excel..