Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 86.0 MPa @# of Cycles 100000 , Temperature 140 °C |
12500 psi @# of Cycles 100000 , Temperature 284 °F |
R = 0.1, 8 Hz, dry |
DSM Stanyl® TW271B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |