Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 52.0 MPa @# of Cycles 1.00e+6 |
7540 psi @# of Cycles 1.00e+6 |
|
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |