Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.89 - 24.1 GPa | 999 - 3500 ksi | Average value: 12.3 GPa Grade Count:43 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |