Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.80 GPa | 986 ksi | ISO 527-2 |
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 20% of glass fibers for industrial parts with high dimensional stab.. |