Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 8.27 - 32.0 GPa | 1200 - 4640 ksi | Average value: 13.0 GPa Grade Count:25 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Modulus of Elasticity | 8.27 - 20.7 GPa | 1200 - 3000 ksi | Average value: 10.9 GPa Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Modulus of Elasticity | 8.27 - 26.2 GPa | 1200 - 3800 ksi | Average value: 17.4 GPa Grade Count:19 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Modulus of Elasticity | 8.27 - 12.4 GPa | 1200 - 1800 ksi | Average value: 10.2 GPa Grade Count:4 |
Overview of materials for Nylon 11 with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ.. |
|||
Modulus of Elasticity | 8.27 - 11.0 GPa | 1200 - 1600 ksi | ASTM D638 |
Premix Premi-Glas® 1200-24 Polyester SMC
(discontinued **) Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa.. |