Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.83 GPa | 701 ksi | std. dev. 0.47 GPa |
Schmelzer Industries Pearlveil 110-20 Fiberglass Veil Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmel.. |