Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.70 - 48.3 GPa | 247 - 7000 ksi | Average value: 13.9 GPa Grade Count:561 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Modulus of Elasticity | 10.0 - 48.3 GPa | 1450 - 7000 ksi | Average value: 22.9 GPa Grade Count:52 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |