Polymer Property : Modulus of Elasticity = 700 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.30 - 4.83 GPa
334 - 700 ksi
Average value: 3.30 GPa Grade Count:26
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Modulus of Elasticity 1.06 - 4.83 GPa
154 - 700 ksi
Average value: 2.84 GPa Grade Count:77
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Modulus of Elasticity 3.03 - 4.83 GPa
439 - 700 ksi
Average value: 4.13 GPa Grade Count:7
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu..
Modulus of Elasticity 2.50 - 4.83 GPa
363 - 700 ksi
Average value: 3.86 GPa Grade Count:12
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..