Mechanical Properties Metric English Comments
Modulus of Elasticity 0.450 - 44.2 GPa
65.3 - 6410 ksi
Average value: 8.04 GPa Grade Count:181
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Modulus of Elasticity 0.450 GPa
65.3 ksi
ASTM D638
Zeus PFA Tubing
PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar..
Modulus of Elasticity 0.450 GPa
65.3 ksi
film; DSM-Method, 50 mm/min
DSM Akulon® F132 PA6
Film Extrusion, High Viscosity
Modulus of Elasticity 0.450 GPa
65.3 ksi
film; DSM-Method, 50 mm/min
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
Modulus of Elasticity 0.450 GPa
65.3 ksi
film; DSM-Method, 50 mm/min
DSM Akulon® F136 PA6
Very High Viscosity, Film Extrusion
Modulus of Elasticity 0.450 GPa
65.3 ksi
film; DSM-Method, 50 mm/min
DSM Akulon® F136-C PA6
Film Extrusion, Very High Viscosity, Lubricated
Modulus of Elasticity 0.450 GPa
65.3 ksi
film; DSM-Method, 50 mm/min
DSM Akulon® F136-C1 PA6
Very High Viscosity, Film Extrusion, Lubricated
Modulus of Elasticity 0.450 GPa
65.3 ksi
Film; DSM-Method, 50mm/min
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Modulus of Elasticity 0.450 GPa
65.3 ksi
AorTech Biomaterials ECSil™ 70D Biomedical Carbonate Silicone Pellets
Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an..
Modulus of Elasticity 0.450 GPa
65.3 ksi
AorTech Biomaterials ECSil™ 70D Biomedical Carbonate Silicone Pellets
Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an..
Modulus of Elasticity 0.450 - 1.50 GPa
65.3 - 218 ksi
Average value: 0.911 GPa Grade Count:51
Overview of materials for High Density Polyethylene (HDPE), Injection Molded