Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 17.5 - 42.7 GPa | 2540 - 6200 ksi | Average value: 28.6 GPa Grade Count:13 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |