Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.89 - 24.1 GPa | 999 - 3500 ksi | Average value: 12.3 GPa Grade Count:43 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 6.89 - 31.8 GPa | 1000 - 4620 ksi | Average value: 13.8 GPa Grade Count:20 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |