Mechanical Properties Metric English Comments
Modulus of Elasticity 3.447 GPa
500.0 ksi
Abatron AboCast 8-14/Abocure 8-14 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.10 ratio (pbw); Gel time, 100 g (3.5 oz.): 63 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°..
Modulus of Elasticity 3.447 GPa
500.0 ksi
Abatron AboCast/AboCure 8109-13
Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45..
Modulus of Elasticity 3.447 GPa
500.0 ksi
Abatron AboCast/AboCure 8109-3
Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140..
Modulus of Elasticity 3.447 GPa
500.0 ksi
Abatron AboCast/AboCure 8109-5
High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications..
Modulus of Elasticity 3.447 GPa
500.0 ksi
Abatron AboCast/AboCure 8109-8
All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi..