Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.17 - 17.9 GPa | 750 - 2600 ksi | Average value: 8.75 GPa Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Modulus of Elasticity | 5.17 - 13.1 GPa | 750 - 1900 ksi | Average value: 8.41 GPa Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Modulus of Elasticity | 5.17 GPa | 750 ksi | ASTM D638 |
ITW Devcon Metal Repair Wear Resistant Epoxy (WR-2), Dark Grey Information provided by ITW Devcon |
|||
Modulus of Elasticity | 5.17 GPa | 750 ksi | ASTM D638 |
ITW Devcon Plastic Steel® Metal Repair 5 Minute® Putty (SF), Dark Grey Information provided by ITW Devcon |
|||
Modulus of Elasticity | 5.17 GPa | 750 ksi | In Tension; ASTM D638 |
Devcon Underwater Repair Putty (UW) Epoxy Emergency Repair ProductsComments: High-performance technology for repairing, patching and rebuilding equipment in habitually wet environments, even under water. Eliminates the need for substrate t.. |
|||
Modulus of Elasticity | 5.17 GPa | 750 ksi | |
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% .. |
|||
Modulus of Elasticity | 5.17 GPa | 750 ksi | |
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°.. |