Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.343 - 0.700 GPa | 49.7 - 102 ksi | Average value: 0.378 GPa Grade Count:11 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Modulus of Elasticity | 0.343 GPa | 49.7 ksi | Molded Sample 2% Secant Modulus |
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for hou.. |