Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.24 GPa | 470 ksi | ASTM D-638 |
Plaskolite Optix® CA - 71 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.24 GPa | 470 ksi | ASTM D-638 |
Plaskolite Optix® CP - 71 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.24 GPa | 470 ksi | ASTM D-638 |
Plaskolite Optix® CP - 71 LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Modulus of Elasticity | 3.24 GPa | 470 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.24 GPa | 470 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 71 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.24 GPa | 470 ksi | ASTM D-638 |
Plaskolite West Optix® CA - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.24 GPa | 470 ksi | ASTM D638 |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |