Mechanical Properties Metric English Comments
Modulus of Elasticity 0.242 GPa
35.1 ksi
Secant; ASTM D638
Huntsman PE1058 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability, excellent strength, good heat sealability, and optics.Applications: Film extrusion: all thin film uses and especiall..
Modulus of Elasticity 0.242 GPa
35.1 ksi
Secant; ASTM D638
Huntsman PE1068 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability even to 1/2 mil; excellent strength, good heat sealability, and good optical.FDA Notes: Conforms to FDA regulation 21..
Modulus of Elasticity 0.242 GPa
35.1 ksi
Secant; ASTM D638
Huntsman PE1356 EVA Film Extrusion  (discontinued **)
3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Modulus of Elasticity 0.242 GPa
35.1 ksi
Secant; ASTM D638
Huntsman PE7011 Profile Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Excellent strength, good machinability, and foaming characteristics.Applications: Extrusion: profile extrusion.FDA Notes: Conforms to FDA regulation 21 CFR 17..
Modulus of Elasticity 0.242 GPa
35.1 ksi
Secant; ASTM D638
Huntsman PE1335 EVA Film Extrusion  (discontinued **)
3.3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Modulus of Elasticity 0.242 GPa
35.1 ksi
Secant; ASTM D638
Huntsman PE1345 EVA Film Extrusion  (discontinued **)
3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Modulus of Elasticity 0.242 GPa
35.1 ksi
Secant; ASTM D638
Huntsman PE 1375 EVA Film Extrusion  (discontinued **)
3.7% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Modulus of Elasticity 0.242 GPa
35.1 ksi
Secant; ASTM D638
Huntsman PE1353 EVA Film Extrusion  (discontinued **)
3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..