Polymer Property : Modulus of Elasticity = 35.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.241 GPa
35.0 ksi
ISO 1184-1983E
LyondellBasell Montell 0300 Polybutene
Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenesApplications: packaging industry, minor additive..
Modulus of Elasticity 0.241 GPa
35.0 ksi
ISO 1184-1983E
LyondellBasell Montell 0800 Polybutene
Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe..
Modulus of Elasticity 0.241 GPa

@Temperature -20.0 °C
35.0 ksi

@Temperature -4.00 °F
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..