Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.39 GPa | 346 ksi | |
Hybrid Plastics Nanoreinforced® POSS® Polyimide Nanoreinforced® POSS® Polyimide is a hybrid nanocomposite that can serve as oxidation resistant and highly bondable form of polyimide. Upon exposure to oxidizing oxygen the POSS® polyimide .. |
|||
Modulus of Elasticity | 2.39 GPa | 346 ksi | Cross; ASTM D638 |
Arlon DiClad 870 PTFE/Woven Fiberglass Laminate Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch.. |