Polymer Property : Modulus of Elasticity = 34.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.240 GPa
34.8 ksi
ISO 5527
Total Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding  (discontinued **)
Low density radical polyethylene made by high pressure process. Temperature profile (°C) for injection molding: 200 to 260Information provided provided by Total Petrochemicals.Total Petrochemicals ..
Modulus of Elasticity 0.240 GPa
34.8 ksi
MD; ISO R527-1
Iran Petrochemical (PCC) 2602TH00 Low Density Polyethylene
LDPE 2602TH00 high clarity film Applications: film, underblankets and films for medical applications.Information provided by Iran Petrochemical Commercial Co.
Modulus of Elasticity 0.240 GPa
34.8 ksi
ISO 5527
Total FE 8000 LDPE blown film
Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired form..
Modulus of Elasticity 0.240 GPa
34.8 ksi
ISO 5527
Total FE 8004 LDPE blown film
Radical polyethylene made by high pressure autoclave process. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former F..
Modulus of Elasticity 0.240 GPa
34.8 ksi
ASTM D638
Zeus THV Tubing
THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity.