Mechanical Properties Metric English Comments
Modulus of Elasticity 3.70 - 20.7 GPa
537 - 3000 ksi
Average value: 6.36 GPa Grade Count:13
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and ..
Modulus of Elasticity 8.27 - 20.7 GPa
1200 - 3000 ksi
Average value: 10.9 GPa Grade Count:6
Overview of materials for PPE/PPO + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 0.586 - 20.7 GPa
85.0 - 3000 ksi
Average value: 2.80 GPa Grade Count:238
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 2.80 - 20.7 GPa
406 - 3000 ksi
Average value: 10.4 GPa Grade Count:84
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..