Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.447 GPa | 500.0 ksi | |
Abatron AboCast 8-14/Abocure 8-14 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.10 ratio (pbw); Gel time, 100 g (3.5 oz.): 63 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |
|||
Modulus of Elasticity | 3.447 GPa | 500.0 ksi | |
Abatron AboCast/AboCure 8109-13 Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45.. |
|||
Modulus of Elasticity | 3.447 GPa | 500.0 ksi | |
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
Modulus of Elasticity | 3.447 GPa | 500.0 ksi | |
Abatron AboCast/AboCure 8109-5 High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications.. |
|||
Modulus of Elasticity | 3.447 GPa | 500.0 ksi | |
Abatron AboCast/AboCure 8109-8 All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi.. |