Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.43 GPa | 497 ksi | ASTM D-638 |
Plaskolite West Optix® CP - 80 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Modulus of Elasticity | 3.43 GPa | 497 ksi | ASTM D638M |
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which tur.. |
|||
Modulus of Elasticity | 3.43 GPa | 497 ksi | ASTM D-638 |
Plaskolite Optix® CP - 80 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |