Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.172 GPa | 460.1 ksi | ASTM D638 |
Ineos Nova 1280 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Modulus of Elasticity | 3.172 GPa | 460.1 ksi | ASTM D638 |
Ineos Nova 2110 General Purpose Crystal Polystyrene
(discontinued **) Moderately high heat resistance, Good balance of strength and ease of processing, USP Class VIApplications: Foam extrusion, Biaxially oriented sheet, Thermoformed drinkware, Molded packagingExposure.. |
|||
Modulus of Elasticity | 3.172 GPa | 460.1 ksi | |
Abatron AboCast 8-13/Abocure 8-13 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 53 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |
|||
Modulus of Elasticity | 3.172 GPa | 460.1 ksi | |
Abatron AboCast 8-18/Abocure 8-18 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |
|||
Modulus of Elasticity | 3.172 GPa | 460.1 ksi | ASTM D638 |
Ineos Nova 1290 High Heat Crystal Polystyrene Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Modulus of Elasticity | 3.172 GPa | 460.1 ksi | |
Lucite International XL Sanitary Ware Acrylic Sheet Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an.. |
|||
Modulus of Elasticity | 3.172 GPa | 460.1 ksi | ASTM D638 |
Ineos Nova 1200 High Heat Crystal Polystyrene Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia.. |
|||
Modulus of Elasticity | 3.172 GPa | 460.1 ksi | ASTM D638 |
Ineos Nova 1204 High Heat Crystal Polystyrene Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia.. |