Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 190 GPa @Temperature 204 °C |
27500 ksi @Temperature 400 °F |
|
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11) TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip General Elgiloy® information: High strength, ductility, fatigue life, and good mechanical properties. Corrosion resistant in numerous environments. Available in strip (currently 0.0015" to 0.075".. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, Heat Treated Heat Treatment 5 hours at 482°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc.. |
|||
Modulus of Elasticity | 190 GPa @Temperature 371 °C |
27500 ksi @Temperature 700 °F |
As-HIP Condition |
Crucible Compaction Metals P/M 625 Corrosion Resistant Alloy P/M 625 (chemically, UNS N06625) is produced by the Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The Crucible powder con.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, Heat Treated Heat Treatment 5 hours at 527°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc.. |
|||
Modulus of Elasticity | 190 GPa | 27500 ksi | (hardened to 62 HRC) |
Bohler-Uddeholm AISI A2 Cold Work Tool Steel Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized byAISI A2 is characterized by: Good machinability High stability after hardening High c.. |
|||
Modulus of Elasticity | 190 GPa @Temperature 399 °C |
27500 ksi @Temperature 750 °F |
hardness of 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel Description: Chromium-molybdenum-vanadium alloyed PM steel. Toolmaking with highly alloyed tool steel means that machining and heat treatment have to be considered more than with lower alloyed grade.. |
|||
Modulus of Elasticity | 190 GPa | 27500 ksi | |
Carlson 2205 (UNS S31803) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Modulus of Elasticity | 190 GPa | 27500 ksi | |
Carlson 2205 (UNS S32205) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Modulus of Elasticity | 189.6 GPa | 27500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Wire The strength and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fatigue life, and.. |