Mechanical Properties Metric English Comments
Modulus of Elasticity 0.620 - 18.6 GPa
89.9 - 2700 ksi
Average value: 8.21 GPa Grade Count:95
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Modulus of Elasticity 9.00 - 18.6 GPa
1310 - 2700 ksi
Average value: 14.0 GPa Grade Count:26
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Modulus of Elasticity 7.58 - 18.6 GPa
1100 - 2700 ksi
Average value: 12.1 GPa Grade Count:79
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..