Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 175 GPa @Temperature 400 °C |
25400 ksi @Temperature 752 °F |
|
Assab Steels 8407 2M Hot Work Steel ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform .. |
|||
Modulus of Elasticity | 175 GPa @Temperature 400 °C |
25400 ksi @Temperature 752 °F |
|
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Modulus of Elasticity | 175 GPa | 25400 ksi | |
Ceradyne Ceralloy® 147-1B Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |
|||
Modulus of Elasticity | 175 GPa @Temperature 400 °C |
25400 ksi @Temperature 752 °F |
|
Assab Steels 8407 SUPREME Hot Work Steel 8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and .. |