Mechanical Properties Metric English Comments
Modulus of Elasticity 17.0 GPa
2470 ksi
ASTM D638
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..
Modulus of Elasticity 17.0 GPa
2470 ksi
DIN 53 457
Albis Plastics Tedur® L V 9200-1 PPS, 60% Glass Fiber/Mineral  (discontinued **)
Mineral-filled Grade with Improved Impact Strength, Low Mold Temp. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Shaft Seals, FlangesProcessing: Injection Molding (M..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1105-8168 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1301-7294/BL PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 19-8373 Polyamide 46, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Improved fri..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 20-7908 Polyphthalamide, with glass fiber and carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1114-0717 PAEK, with carbon fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1105/XCF/15-S PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Modulus of Elasticity 17.0 GPa
2470 ksi
ISO 527-1/-2
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
Modulus of Elasticity 17.0 GPa
2470 ksi
DIN 53 457
Albis Plastics Tedur® P 9529 PPS, ~55% Glass Fiber/Mineral (black only)
Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Lamp Holders, Lamp SocketsProcessing: Inj..
Modulus of Elasticity 17.0 GPa
2470 ksi
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified