Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.50 - 24.1 GPa | 508 - 3500 ksi | Average value: 7.16 GPa Grade Count:21 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Modulus of Elasticity | 4.14 - 24.1 GPa | 600 - 3500 ksi | Average value: 10.1 GPa Grade Count:55 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Modulus of Elasticity | 6.89 - 24.1 GPa | 999 - 3500 ksi | Average value: 12.3 GPa Grade Count:43 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 7.65 - 24.1 GPa | 1110 - 3500 ksi | Average value: 15.5 GPa Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and.. |