Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 0.161 GPa @Temperature -100 - 150 °C |
>= 23.4 ksi @Temperature -148 - 302 °F |
Average value: 2.53 GPa Grade Count:1 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |