Polymer Property : Modulus of Elasticity = 22.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.153 GPa
22.2 ksi
Molded Sample 2% Secant Modulus
Dow LDPE 4012M Low Density Polyethylene
DOW LDPE 4012M resin is a broad molecular weight distribution homopolymer designed to provide good impact strength, excellent flexibility and high stress crack resistance for housewares, toys and ge..