Polymer Property : Modulus of Elasticity = 1380 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 9.50 - 30.0 GPa
1380 - 4350 ksi
Average value: 18.7 GPa Grade Count:19
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 1105-8053/EM/BL PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 50-0833 Polycarbonate, with carbon fiber and glass fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Electrical..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 50-8025 Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 6-7433 Polyamide 12, with carbon fiber, hydrolysis resistant
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15 Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/SI/2-2 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 1105-7720/BE PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® PC-50/GF/30/TF/15/ BK Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Modulus of Elasticity 9.50 GPa
1380 ksi
ISO 527-2
Tisan TISESTER® 30% Glass Fiber Reinforced and heat Stabilized Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
Modulus of Elasticity 9.50 GPa
1380 ksi
ISO 527-2
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
Modulus of Elasticity 9.50 GPa
1380 ksi
ISO 527-2
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
Modulus of Elasticity 9.50 GPa
1380 ksi
ISO 527
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry)
Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Modulus of Elasticity 9.50 GPa
1380 ksi
ISO 527
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry)
Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Modulus of Elasticity 9.50 GPa
1380 ksi
ISO 527-2
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT
Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so..
Modulus of Elasticity 9.50 GPa
1380 ksi
ISO 527
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade.
Modulus of Elasticity 9.50 GPa
1380 ksi
ISO 527
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
Modulus of Elasticity 9.50 GPa
1380 ksi
Lehmann & Voss LUVOCOM® 1105-7173/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..