Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.945 GPa | 137 ksi | ASTM D638 |
Huntsman Rexell® H2110 Injection Molding LLDPE
(discontinued **) Linear-low high density injection molding.Features: Good toughness, ESCR.Applications: Industrial and consumer pails, general purpose molding.Information provided by Huntsman Corporation |