Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 86.0 GPa | 12500 ksi | |
Piezo Kinetics 700 Lead Zirconate Titanate Piezoelectric This material has low dielectric constant, high QM, high shear coupling coefficient, good temperature stability and low aging characteristics. Common use of this material is in delay lines and accel.. |
|||
Modulus of Elasticity | 86.2 GPa @Temperature 649 °C |
12500 ksi @Temperature 1200 °F |
|
Latrobe Lescalloy® M50 VIM-VAR High Performance Bearing Steel LESCALLOY M50 VIM-VAR steel is a through-hardening grade with high hardness and high compressive strength at elevated temperatures. It is produced exclusively as a double vacuum melted produced usi.. |
|||
Modulus of Elasticity | 86.0 GPa | 12500 ksi | |
Schott N-BAF52 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 86.0 GPa | 12500 ksi | ASTM C-1259 |
Schott Nextrema® 712-6 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Modulus of Elasticity | 86.0 GPa | 12500 ksi | ASTM C-1259 |
Schott Nextrema® 724-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Modulus of Elasticity | 86.0 GPa | 12500 ksi | |
Schott N-SF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 86.0 GPa | 12500 ksi | |
Schott N-SK14 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 86.0 GPa | 12500 ksi | |
Schott P-SF8 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 86.0 GPa | 12500 ksi | |
AGY VeTron® Glass Fiber Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance.Information provided by AGY Holding Corp. |