Mechanical Properties Metric English Comments
Modulus of Elasticity >= 0.800 GPa
>= 116 ksi
ISO.178 DN.53452
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500
PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce..
Modulus of Elasticity 0.800 GPa
116 ksi
ISO 178
Premix Thermoplastics PRE-ELEC® PE 1295
PRE-ELEC PE 1295 is a dissipative thermoplastic compound based on PE-HD. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance bet..
Modulus of Elasticity >= 0.800 GPa
>= 116 ksi
ISO.178 DN.53452
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500
PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce..
Modulus of Elasticity 0.800 GPa
116 ksi
ISO 527
GEHR Plastics PE-UHMW-ELS Polyethylene  (discontinued **)
Polyethylene offers resistance to almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature of HDPE is from -58 °F to +1..
Modulus of Elasticity 0.800 GPa
116 ksi
1 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer  (discontinued **)
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General ..
Modulus of Elasticity 0.800 GPa
116 ksi
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers..
Modulus of Elasticity 0.800 GPa

@Temperature 23.0 °C
116 ksi

@Temperature 73.4 °F
MD/TD; ASTM D638
Mapal Plastics Maplon PAPER MATCH Polypropylene Sheet
Paper match is a multi layer graphic sheet. The core layer is a high rigidity PP. The skin layers are high field polyolefine. The surface bonds easily to inks and have some absorbing capacity.Main a..
Modulus of Elasticity 0.800 GPa
116 ksi
ISO R527
Arkema Group Orgalloy® LE 60XV Polyamide 6 Alloy
Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Modulus of Elasticity 0.800 GPa
116 ksi
Average value: 0.800 GPa Grade Count:3
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..
Modulus of Elasticity 0.800 - 9.31 GPa
116 - 1350 ksi
Average value: 2.08 GPa Grade Count:120