Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 77.9 GPa | 11300 ksi | |
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet.. |
|||
Modulus of Elasticity | 77.9 GPa | 11300 ksi | Parallel to pressing direction |
Momentive Performance Materials HBN Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Modulus of Elasticity | 77.9 GPa | 11300 ksi | Effective Modulus |
Hardwire 3x2-23-12 High Density Composite The 3x2 Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3x2 wire cord is made by twisting 5 individual wire together - three straight filam.. |
|||
Modulus of Elasticity | 78.0 GPa | 11300 ksi | |
Schott N-SK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 78.0 GPa | 11300 ksi | Virgin Filament |
Saint-Gobain Quartzel® Fused Quartz Textiles Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava.. |
|||
Modulus of Elasticity | 78.0 GPa | 11300 ksi | |
Schott N-KZFS4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 77.6 GPa | 11300 ksi | |
Mateck Window Grade Zinc Selenide, ZnSe Optical Crystals |