Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 73.1 GPa | 10600 ksi | |
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m.. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | |
Piezo Kinetics 804 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type III, it is specifically used as a driver that exhibits low losses under extreme driving conditions and has a high Q. PKI 804 is well suited for medical applications.Elastic Comp.. |
|||
Modulus of Elasticity | 72.9 GPa | 10600 ksi | |
Schott D 263 Thin Borosilicate Glass D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang.. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | |
Schott Glass 8625 Biocompatible Glass Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S.. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | |
Schott N-BAK1 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | |
Schott N-FK51A Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | compression |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | compression |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | compression |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | compression |
Constellium Certal® SPC Aluminum Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man.. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | compression |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |
|||
Modulus of Elasticity | 73.0 GPa | 10600 ksi | |
Schott DUROBAX® clear Neutral Glass Tubing Neutral glass tubing, chemically highly resistant Syringes, cartridges, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is.. |