Polymer Property : Modulus of Elasticity = 1.86 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.86 GPa
270 ksi
ASTM D-638
Plaskolite Optix® CA - 2000 HF-4-2 High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Modulus of Elasticity 1.86 GPa
270 ksi
ASTM D-638
Plaskolite Optix® CA - 2000 High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Modulus of Elasticity 1.86 GPa
270 ksi
ASTM D-638
Plaskolite Optix® CP - 1000 IG High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Modulus of Elasticity 1.86 GPa
270 ksi
ASTM D-638
Plaskolite West Optix® CP - 1000 IG High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Modulus of Elasticity 1.86 - 3.10 GPa
270 - 450 ksi
Average value: 2.80 GPa Grade Count:8
Overview of materials for Acrylic, High Flow, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app..
Modulus of Elasticity 1.86 GPa
270 ksi
Tangent; ASTM D790
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade  (discontinued **)
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Modulus of Elasticity 1.86 - 8.96 GPa
270 - 1300 ksi
Average value: 2.71 GPa Grade Count:14
Overview of materials for Nylon 612 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app..
Modulus of Elasticity 1.86 GPa
270 ksi
ASTM D-638
Plaskolite West Optix® CA - 2000 HF-4-2 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Modulus of Elasticity 1.86 GPa
270 ksi
ASTM D-638
Plaskolite West Optix® CA - 2000 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..