Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0100 GPa | 1.45 ksi | |
Nanosonic Metal Rubber™ Metal Rubber™ is a unique self-assembled nanocomposite material that combines the high electrical conductivity of metals with the low mechanical modulus of elastomers. Self-assembly processing allo.. |
|||
Modulus of Elasticity | 0.0100 GPa | 1.45 ksi | DMA |
Lord Adhesives Thermosetâ„¢ MS-330 Silicone Board Level Encapsulant LORD Thermosetâ„¢ MS-330 encapsulant is a one component silicone specifically designed for use on high-frequency devices including Bluetooth applications. This silicone encapsulant offers excelle.. |
|||
Modulus of Elasticity | 0.0100 GPa | 1.45 ksi | Calculated; ASTM D412 Method A |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Modulus of Elasticity | 0.0100 GPa | 1.45 ksi | |
AorTech Biomaterials ECSil™ 75A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Modulus of Elasticity | 0.0100 - 0.0200 GPa | 1.45 - 2.90 ksi | TM-019E |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |
|||
Modulus of Elasticity | 0.0100 GPa | 1.45 ksi | |
AorTech Biomaterials ECSil™ 75A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Modulus of Elasticity | 0.0100 - 0.0200 GPa | 1.45 - 2.90 ksi | TM-019E |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |