Polymer Property : Modulus of Elasticity = 0.400 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.400 GPa
58.0 ksi
ISO 178
Premix Thermoplastics PRE-ELEC® PE 1313  (discontinued **)
PRE-ELEC PE 1313 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 13..
Modulus of Elasticity 0.400 - 3.50 GPa

@Temperature 40.0 - 150 °C
58.0 - 508 ksi

@Temperature 104 - 302 °F
Average value: 1.37 GPa Grade Count:5
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Modulus of Elasticity 0.400 - 9.20 GPa

@Temperature 60.0 - 150 °C
58.0 - 1330 ksi

@Temperature 140 - 302 °F
Average value: 2.28 GPa Grade Count:5
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Modulus of Elasticity 0.400 - 10.0 GPa
58.0 - 1450 ksi
Average value: 6.07 GPa Grade Count:53
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Modulus of Elasticity 0.400 GPa

@Temperature 23.0 °C
58.0 ksi

@Temperature 73.4 °F
MD/TD; ASTM D638
Mapal Plastics Maplon Type H Polypropylene Sheet
Properties : Good resistance to low temperatures, Moderate stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printing.Applications : Stationery, Printing..
Modulus of Elasticity 0.400 GPa
58.0 ksi
BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue..
Modulus of Elasticity 0.400 - 0.800 GPa

@Temperature 100 - 100 °C
58.0 - 116 ksi

@Temperature 212 - 212 °F
Average value: 0.600 GPa Grade Count:2
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..